Class 3 coating (AS 3566 fasteners)

Class 3 (AS 3566.2) is the corrosion classification for fasteners in moderate-exposure environments. Required for treated timber, wet areas, mild coastal.

Ask Chalkline about this →

A Class 3 coating in residential construction refers to the corrosion resistance classification under AS 3566.2:2002 for self-drilling screws and other fasteners. The standard defines five classes (Class 1 through Class 5) of increasing corrosion resistance, each suited to a defined exposure environment. Class 3 is the moderate-exposure tier required for treated-timber fixings, wet-area work, and mild-coastal applications.

The AS 3566.2 corrosion classes:

ClassExposureTypical coating
Class 1Internal dryStandard zinc-plated (electroplated, 5-8 microns)
Class 2Internal damp, mild externalMechanical zinc, HDG light (10-15 microns)
Class 3Treated timber, wet areas, mild coastalHDG full (40-100 microns) or duplex zinc/aluminium coatings
Class 4Severe industrial, marineStainless 304 or specialised coating
Class 5Severe marine, splash zoneStainless 316

A Class 3 coating typically means hot-dip galvanised (HDG) to a minimum 40-100 microns of zinc, or equivalent zinc/aluminium coating (e.g. Zincalume-coated steel in some applications).

Where Class 3 is required:

  • Fastening into treated timber (H2, H3, H4): the copper and chromium actives in ACQ and CCA are aggressive on standard zinc-plated fasteners. Class 3 (HDG) is the standard residential requirement.
  • Wet-area fixings: bathroom, laundry, toilet trim, where condensation and water spray reach the fastener. Class 3 minimum.
  • Mild-coastal areas (within 5 km of moderate marine): residential roofing fasteners, fascia fixings.
  • External non-marine work: cladding, fascia, gutter brackets in standard inland environments.

Where Class 2 is acceptable (lower spec): internal framing, dry roof framing, internal joinery in dry environments. Don’t substitute Class 2 for Class 3 in treated-timber applications; the actives will corrode through within years.

Where Class 4 or Class 5 is required:

  • Severe marine: within ~1 km of breaking surf. Stainless 304 or 316.
  • Pool decks and water-feature framing: continuous salt or chlorine exposure.
  • High-end marine residential where 30+ year service life is expected.

Identifying Class 3 fasteners on site:

  • Packaging label: “AS 3566 Class 3” or “Class 3 HDG” printed on the box.
  • Head colour: HDG fasteners are silvery-grey (sometimes with a slight roughness from the dip); zinc-plated standard fasteners are smooth shiny silver.
  • Manufacturer catalogue: spec class for each product line.

Common builder errors:

  • Class 2 in ACQ-treated decking: rust streaks within years, joist-board bond fails as the screw corrodes.
  • Class 3 in severe marine: works for ~10 years then fails; should have been stainless.
  • Mixed classes on the same job: aesthetic continuity broken; inconsistent service life across the build.
  • Confusing Class 3 with stainless: Class 3 is HDG zinc; stainless is Class 4+. Different metal, different cost (stainless typically 3-5x HDG cost).

For builders:

  1. Spec fastener class in the contract scope by application zone (internal, treated timber, external, coastal).
  2. Don’t buy cheaper standard zinc for treated-timber work. The 30-50% cost saving on screws translates to 10-20% rework cost on the building when the joist starts moving.
  3. Confirm packaging at delivery: a yard mix-up can put Class 1 or 2 in the bag labelled “for treated decking”. Read the box, not just the sticker.

Also known as: AS 3566 Class 3, Class 3 fastener, Type 3 corrosion class (informal).